NEW: Onshore Inspections
The Flux
A robust handheld system for corrosion detection and 3D mapping of unpiggable pipelines.
Discover the Flux
NEW: Onshore Inspections
A robust handheld system for corrosion detection and 3D mapping of unpiggable pipelines.
Discover the Flux →
NEW Service
Know how fast every coating defect corrodes, in µm/year, validated against excavations.
See how it works →
FREE: Whitepaper
How CMI separates protected steel from actively corroding steel, without excavation.
Download →The probability of detection (POD) states how likely an inspection method is to find a defect of a given type and size. It is the first of the performance figures by which inspection systems are specified and qualified, next to the probability of identification, the sizing accuracy and the false call rate. For in-line inspection, API Standard 1163 sets the framework.
On this page
At a glanceThe figuresProofAbove-ground methodsCMIFAQ
| Stands for | Probability of detection |
| States | The probability that an anomaly is detected, for each anomaly type and above a stated detection threshold |
| Companion figures | Probability of identification (POI), sizing accuracy, false calls |
| Framework for in-line inspection | API Standard 1163, In-line Inspection Systems Qualification |
| Proven by | Tests on known defects, and comparison of inspection results with excavation findings |
| Blind test | The inspection team does not know where the defects are |
A performance specification is a claim until it is validated. API 1163 covers the qualification, selection, reporting, verification, validation and use of in-line inspection systems, and it asks for performance specifications to be established, documented and validated.
Validation compares what the inspection reported with what is really there. This can be a test piece with fabricated defects, or excavations on the pipeline where the findings are measured in the ditch.
A small number of trials proves little. Statistical methods translate the number of detections and misses into a POD with a confidence level.
A blind test adds one condition: the inspection team does not know where the defects are, or how many there are. Only then does the test also show false calls.
API 1163 is written for in-line inspection. For above-ground methods, operators ask the same questions: what is detected, how reliably, and with how many false calls. The answers come from blind tests and from excavations.
EMPIT has carried out more than 30 blind tests of Current Magnetometry Inspection (CMI) with operators. In each of them, only the operator knew the position of the defects.
One of them is published in detail. On a 45 m test spool with three diameters, buried 1.2 to 1.5 m deep, an independent third party fabricated 13 blind defects and one simulated repair. CMI found all 13 from the surface. Nothing was reported where no defect had been fabricated, and no indication was raised at the simulated repair.
The test also documents a limit. Defects closer together than the 2 m spatial resolution of the method were reported as one combined feature.
In the field, the DVGW research project NEMEK compared methods on operating pipelines. Across 37 excavations, CMI assessed the effectiveness of cathodic protection correctly in 94.6% of cases. These are test results, not a POD figure in the sense of API 1163. See 13 of 13 Defects Found in a Blind Test and the NEMEK results.
Probability of detection: the probability that an inspection finds an anomaly of a given type above a stated detection threshold.
POD describes whether an anomaly is detected at all. POI, the probability of identification, describes whether it is then correctly identified.
An indication that the inspection reports where no defect exists. False calls cost excavations, so they are part of the performance of a method.
A test in which the inspection team does not know the position or number of the defects. It shows detection and false calls under realistic conditions.
If you want to know what an above-ground inspection would show on your line, send us the length, diameter and location of the pipeline. We will tell you whether CMI fits and what a pilot section would look like.
Sources
Read more
19. August 2026
21. February 2026
We use cookies to give you the best possible experience on our website and to improve our communication with you. We only use the data for which you have given us your consent, with the exception of the cookies that are absolutely necessary for the functionality of this website. For more information, please see our privacy policy. Make your choice here:
You can change your consent at any time by clicking on the Cookie Settings link in your footer.
Protects against cross-site request forgery attacks.
Saves the current PHP session.
Cookie from Google for website analytics. Generates statistical data about how visitors use the website. https://policies.google.com/privacy?hl=de